Photopolymer dual cure direct emulsion for the broadest range of applications.

MAGNA/CURE® UDC-HV
UDC-HV dual cure emulsions are designed for the
widestrange of imaging applications. UDC-HV
provides these additional benefits:

• Fast exposure with excellent image quality


• Hard, durable stencils, resistant to the
widest range of inks and additives
• Superior mesh adhesion
• Lightening fast washout and easy reclaim
• High viscosity allows coating on low or

CHROMALINE DUAL CURE EMULSION


high mesh counts

Magna/Cure® UDC-HV direct emulsion allows screen


makersto obtain remarkable image quality and exception-
ally durable stencils. In addition, UDC-HV's high viscosity
allows for excellent coating on low or high mesh counts.

For use with solvent, UV and plastisol based inks.

MATERIALS Viscosity: 5300 CPS (unsensitized)


REQUIRED RECOMMENDED Other: Available upon request
Exposure unit Drying cabinet Standard Sizes: Quart, Gallon, 3.5 Gal., 50 Gal. Drum
Washout sink Pressure washer
Clean work area Chromaline Exposure STORAGE
Scoop coater Calculator Sensitized UDC-HV emulsion has a shelf life of 4 to 6 weeks
at room temperature (60 to 80°F) or longer when refrigerated.
CHEMICALS To maximize sensitized shelf life use only
REQUIRED RECOMMENDED distilled water to dissolve diazo sensitizer.
Chroma/Clean™ Chroma/Haze™
mesh degreaser haze remover Protect from freezing. UDC-HV is not freeze/ thaw stable.
Chroma/Strip™ Chroma/Brade™ Freezing during shipping may result in clear gel spots which
screen reclaimer mesh abrader may resemble pinholes.

SAFETY AND HANDLING Coated, unexposed screens can be stored as long as one
Avoid contact with skin and eyes. month in a clean, cool, dry and completely dark area.
Refer to MSDS for further information.
Expiration date. Always check the expiration date on
SPECIFICATIONS sensitizer bottle to assure freshness.

Exposure: Fast (see reverse)


Solids: 35% (unsensitized)

Chromaline Screen Print Products


SCREEN PRINT PRODUCTS 4832 Grand Ave. Duluth, Minnesota 55807 USA Tel 218-628-2217
Fax 218-628-3245 Web www.chromaline.com E-mail sales@chromaline.com

AN IKONICS COMPANY ISO 9001 CERTIFIED NASDAQ LISTED: IKNX


MAGNA/CURE®

UDC-HV
INSTRUCTIONS
DEGREASE RECLAIM
Using Chroma/Clean™ mesh degreaser, Apply Chroma/Strip™ screen
Work work up a lather on both sides of mesh. reclaimer to both sides of screen.
under Flood screen and frame thoroughly with Scrub area to be reclaimed with a
yellow water, then dry. stiff nylon brush to ensure entire
lights.
surface is wet and let it work a few
MIX moments until stencil begins to dis-
Mix emulsion and sensitizer according to instructions on solve. Remove stencil residue with
bottle. Let emulsion stand at least two hours before using. pressure washer, then rinse with
water, thoroughly flooding screen
COAT and frame.
Fill scoop coater with room temperature
emulsion. Slowly apply first coat to print EXPOSURE GUIDELINES
side. Then coat squeegee side with one Note: Exposure times are suggested only as a guide.
to three coats depending upon thickness Use the Chromaline Exposure Calculator to determine
required. If thicker stencil is required, optimal exposure times. Individual exposure times
additional coats may be applied to print may vary depending upon equipment used, bulb age,
side after initial drying of stencil. Be sure and other shop conditions.
to dry thoroughly between coats.
SUGGESTED MINIMUM
DRY Exposure Guidelines
Thoroughly dry screen in horizontal
position, print side down, using Mesh Time
a dark, clean drying cabinet. 158 mesh TPI
Temperature should not exceed 60 - 90 sec.
(62 cm)
110°F (43°C).
230 mesh TPI
45 - 60 sec.
EXPOSE (90 cm)
Place emulsion side of photopositive 305 mesh­TPI
30 - 45 sec.
in contact with print side of screen. (120 cm)

DEVELOP Exposure times were determined using the Chromaline Exposure


Calculator. Exposure times were set for a 5KW unit at 40" from the
Gently spray both sides of screen frame. All screen mesh was yellow in color. Screens were coated wet
with tepid water, wait 30 seconds on wet, once on print side and twice on squeegee side.
then gently wash print side of the
screen until image is fully open.
AVOID FAILURE: Dual cure emulsions have a very wide
Rinse both sides thoroughly. Dry exposure latitude. Underexposed stencils often appear
screen completely and you are acceptable, but premature breakdown can occur on the
ready to print. press. When determining exposure speed, always
overexpose your test stencil. Then, using the Chromaline
Exposure Calculator, reduce exposure time until acceptable
image quality is achieved. This will help assure good durability.