Sunteți pe pagina 1din 12

Sl.

No
1

3
4

7
8
9
10

11

12
13

14
15
16
17

18

19
20
21
22
23
24
25
26
27
28
29
30

31
32

33

34
35
36
37
38
39
40
41

42
43

44

45
46
47
48
49
50
51
52
53
54
55
56
57
58
59
60
61

62
63
64
65

66
67
68
69

70
71
72
73
74
75
76
77

78
79
80
81
82
83
84
85
86
87
88
89
90

91
92
93
94
95
96
97
98
99
100
Questions
How did low carbon weldable SS316L differ from the ordinary stainless steel.
What is required for a Inspection engineer or Inspector(.A, Being well informed, Impartial B, should have good welding experien
with all)
When you find a welding repair in the welding whom to report for rectification(A, to the welder his welder no mentioned near t
Next person to the welder, D,Welder foreman, D, Project co-coordinator.)
What is PMI

What is importance of essential Variable in WPS

Why Maximum inter pass temperature to follow when doing austenitic stainless steel.

What is NACE MR 0175

What is the additional test apart from hardness test required as per NACE MR 0175
What is acronym of SAW
What is acronym of FCAW

What is WPS

WHAT IS PQR

What is 1 mill surface roughness unit

What is carbon equivalent

If a welder is approved in 6G position what are the positions he is qualified to do welding?


   How welding is performed in 3g position.

What are the mechanical test shall be conducted for toughness test

What is HAZ

What are the precautions to be taken for welding low hydrogen electrode?

Hydrogen in the steel creates a induced crack or corrosion


What is ASME SEC V
Porosity will be better deducted in which method RT or UT
Twhich method is best for the laminar defect parallel to surface
What is welding toe
What is auto genius welding
1 degree how many radians
To weld ss 304 with carbon steel at root which electrode shall be used.
When doing root welding of joint were back side welding is not possible which welding process is ideal?
What is difference between discontinuity and defect

What is the international standard for quality assurance

What is the deference between DCEP and DCRP

What are 5 important things you will check in material test certificates.

What is purpose of pre heating

What is the purpose of PWHT

If a change in PQR essential variable re qualification is required or not


What are the different types of defects shall be noted in welding
What are different types of hardness testing
What ANSI standard shall be followed for pipe welding procedure and welder qualification test
In a metal were you find melted dots by electrical contact on the surface which is happened due to what
Is it possible to arrive tensile strength from the hardness of the material
Mention different types plate welding position

What are the types of weld and describe each

Write 2 attributes of flattening test of weld

 Define SMAW

Define GTAW

What are the two test in electric arc welding


What are the different types of steel making process
If Carbon percent is less in material then the weld ability is increased or decreased
What do you mean by Gr. 60 in ASTM A 516 GR. 60
What is P no parent metal no.
What is F no filler metal no.
What is A no AWS classification
What mechanical test qualifies the welder
What is the NDT method used to deduct crack in welding
What is the 3 type of metal transfer in GMAW
Mention types of metal transfer in SMAW
Where is inter pass temperature to be checked
3 attributes of tensile testing
In TIG welding austenitic stainless steel pipe, what is the purpose of argon gas backing?
What you will check/verify in Raw material test certificates?

What is the standard to be referred for castings visual inspection?

What is Difference between Hardness and Toughness?

What is the standard for welding rods Electrodes and filler metals?
Which type of electrode we are using in GTAW process?
Why we are baking the electrodes?

What is the Procedure for Fit-Up inspection?

How much weld bead width we can allow?


If welder made test by 14 mm thickness, what is his thickness range qualified?
What is carbon % in low carbon steel?

What is meaning for SAES,SAEP and SAMSS?

What is the standard for Structural steel fabrication?


Where we can use E-6010 type electrode?
Which type of welding process we are using in field/fabrication shop?
What is the standard for welding and Brazing Qualifications?
What is the standard for Process (or) Plant piping systems?
What is the standard for Welding symbols?
How much root face are allowed?

What are the essential variables for GTAW process?

If welder made test by 2’’ dia, what is his range qualified?


What is the interpass temperature for carbon steel materials?
What is the standard for liquid Petroleum Transportation piping systems?
What is the Code for Welding of Pipelines and Related facilities?
What is the specification/classification for carbon steel Electrode?
What is the specification/classification for carbon steel filler wire?
What is the hydrotest pressure?
What is the drying procedure procedure for Low hydrogen electrodes?
What are the defects we can find in visual Inspection?
What is the Pressure gauge requirement for hydro test
If the root gap is found lees than requirement during fitup inspection what you will do?
What is the most important thingbefore start welding of Clad material ?

What is interpass temperature?

Which NDT method is suitable to detect lack of side wall fusion?


When a welder qualified in 5G pisition ,which position he can weld?
What are the four types of weld joints.
what is the purpose of spot facing or back facing of Flange holes?
What is the advantage of Magnetic particle testing over DP testing
A weld procedure is qualified in 1G position,this procedure can be used which welding positions
Double wall double image RT technique is used for which weld joints
For MT examination Prod technique the magnetising current required depends on
what is the maximum defect permitted on the convex surface of a welder qualification bend test specimen after bending
Answer
Low carbon & alloying element Molybdenum

Should be impartial

Project Coordinator.
Positive material Identification, To detect the alloying elemenets of the component with Poratble spectro analyser
In base metal thickness, P-number, dia of pipe, pre, post weld heat treatment
In filler metals F,A-numbers, dia
Due to sensitisation(Chromium carbide formation at 500-800 degree Celsius will happen if the temperature maintained for a
reasonable time)
National association of corrosion engineers MR01-75 is recommended practice for sour service. To be followed for suitable
material of construction for sulfide stress corrosion cracking.
HIC
Submerged Arc Welding
Flux Cored Arc Welding

A Welding Procedure Specification (WPS) is the formal written document describing welding procedures, which provides directi
to the welder or welding operators for making sound and quality production welds as per the code requirements
Procedure Qualification Record which provide testing result of welded sample of procedure and shown actual reading of
parameter.
Surface roughness average is 1 micro inch

Carbon Equivalent(CE) is used for rating weldability of ferritic low alloy steel.It takes into account that the equivalent additive
effects of carbon and other alloying elements on a particular characteistic odf steel CE- C=MN/6+(Cr+Mo+V)/5 +(Cu+Ni)/15
All positions
Vertical position
Impact tests
Heat affcted zone of parent metal near welding which is not melted and has had its microstructure and properties altered by
welding

1. Joint surface to be cleaned properly


2.Electrodes are to be baked and tried before use.
3.Pre heating to be ensured as per WPS requirement.
Crack
ASME Code for Non destructive tests
RT
UT
Bountry between weld face and parent metal or between runs.
Autogenous Weld - A fusion weld made without filler metal. Eg.Resistance welding
0.175radian ( 1xpi/180)
E 309
GTAW
Discontinuity is an objective lack of material, an interruption in the physical consistence of a part
Defect-An irregularity or flaw whose total size, shape, orientation, location, or properties do not meet specified acceptance
criteria and are rejectable
ISO 9001

DCEP- Direct Current Electrode Positive(Reverse Polarity) DCEN- Direct Current Electrode Negative(Straight Polarity)

To slow the cooling rate of the weld and the base material, resulting in softer weld metal and heat affected zone microstructure
with a greater resistance to fabrication hydrogen cracking.
Welding process can inadvertently weaken equipment by imparting residual stresses into a material,In order to ensure the
material strength of a part is retained after welding PWHT is being done .
Yes, required.
Porosity,slag inclusion,lack og fusion,Incomplete penetration,spatter,Crack,Stray arc,
Brinell hardness,Rackwell Hardness, Vickers Hardness
ANSI B 31.3
Sray arcs are due to , Un insulated Electrode handle contact with parent metal /Wrong manipulation electrode
Yes, We arrive the tensile value through conversion
1G(Down hand), 2G(Horizontal),3G (Vertical) & 4G(Overhead)

1.Fillet Welds-A fillet weld joins two surfaces at an approximate right angle to each other
2.Groove Welds-The groove weld refers to beads that are deposited in a groove between two members to be joined.
3.Surfacing Weld or Over lay weld-This type of weld is used to build up surfaces or replace metal on worn surfaces
4.Slot Weld-
Ductility & Plasticity

Shielded Metal Arc Welding is a manual arc welding process that uses a consumable electrode coated in flux. An electric curre
either alternating current or direct current, forms electric arc between the electrode and the metals to be joined. As the weld i
laid, the flux coating of the electrode disintegrates, providing a shielding gas and a layer of slag, both of which protect the weld
from contamination until it cools
An arc welding process that produces coalescence of metals by heating them with an arc between a tungsten electrode
(nonconsumable) and the workpiece. Shielding is obtained from an inert gas. Also called TIG welding.
Destructive and Non destructive testing
Basic Oxygen process,Electric Arc Furnace
Will be increased.
Gr.60 referes minimum tensile strength 60 Ksi
P – is base metal grouping Number
F- is filler metal grouping Number.
A – is electrode chemical analysis number
Bend test
Radiographic test
Dip transfer,Spray tranfer and Globular transfer
Drops,spray and globular
75 mm minimum from both end of the Joint
Tensile Strength,Yield Strength & Elongation
To prevent oxidization of root weld.
Type of certificate (3.1 or 3.2), manufacturer, Purchase order number,Specification & Grade,Mechanical test,Chemical test, Hea
no,Lot no and Heat treatment
MS-SP-55

Hardness is a measure of how resistant solid matter is to various kinds of permanent shape change when a compressive force i
applied.
Toughness is the ability of a material to absorb energy and plastically deform without fracturing.
ASME Sec.II part C
Non-Consumable Tungston Electrode
To remove the moisture content from the Electrodes.

Base metal classification,cleaning,Alignment,root gap,root face,bevel angle , mismatch (or) overlap and dimensions.
Max 3 times of electrode diameter.
He has qualified unlimited thickness.
Max 0.30 %

Saudi Aramco Engineering Standards


Saudi Aramco Engineering Procedures
Saudi Aramco Materials System Specification.
AWS D 1.1
we can use at root pass for deep penetration
Fusion welding
ASME Sec-IX
ASME B 31.3
AWS A2.4.
As per WPS (or) 0.8 to 1.6 mm

In Base Metal thickness, P-number, dia of pipe, pre, post weld heat treatment… In Filler Metals F, A-numbers,dia of filler metal
He has qualified 1’’-dia and above.
Max 315’C
ASME B31.4
API 1104
AWS 5.1/E-XXXX
AWS 5.18/ER70-Sx
1.5 Times of design pressure
260 to 430 degree temperature.baking for two hours
Porosity,Undercut,Surface crack (HIC),Side wall fusion on fusion boundary
Pressure gauge-(30days calibration valid, range 1.5 to 2 times test pressure)
Advise to open wider gap by gouging /grinding
Pre heating

In a multipass welding,the welding temperature of the weld area in between weld passes in known as Interpass temperature
UT
1G,2G & 5G
Butt joints, Tee joints, lap joints,Corner joints
To ensure proper seating surface for washer and nut
It can detect sub surface defects
All positions
Tube joints with outer diameter less than 3.5"
Prod spacing and Thickness of item .