Sunteți pe pagina 1din 4

MARATHON GROUP

RMC PARAMETER
1 Site Name

2 Grade of Concrete

3 Special Requirment if any (like SCC, Fibre, Temp.Control)

4 Member Details

Structural member

Non structural member

5 Height of Pumping

a) Upto ground level b) Upto 50 meter

c) Upto 100 meter d) Above 100 meter

6 Type of shuttering used

7 Microfine required to be used

8 Combined flakiness & elongation index of aggregates It should not exceed more than 40%.

9 For raft, combination of mix used (e.g. OPC+Fly ash or OPC+GGBFS)

1) Peak temperature of concrete should not exceed 70 oC.


### For Mass concrete 2) Thermal gradient within the concrete mass should not exc
3) For mass concrete, it is advisable to design concrete for 56

### Modulus of Elasticity of concrete It should be as per IS 456 Clause 6.2.3.1 for normal density c

### Minimum cement (incl. flyash, ggbs & other cementitious) content

### Maximum Water to Cement (incl. flyash, ggbs & other cementitious)
ratio

1) Chloride content of concrete should not exceed :-


a) 0.4 kg/m3 for Steam cured or pre stressed concrete,
### Limits of Chloride & Sulphate content in concrete b) 0.6 kg/m3 for Reinforced cement concrete &
c) 3.0 kg/m3 for concrete not containing embeded meta
2) Sulphate content of concrete should not exceed 4% by ma
Fresh Concrete Properties

1 Slump Flow

2 On site, Slump/Flow required

3 During trials, Slump/Flow required

Initial Slump/Flow

Final Slump/Flow

8 Retention period 3 hour or 4 hour

9 Others requirment, if any

Filling ability , Passing ability, Segregation


Like, SCC Resistance

Hardened Concrete Properties

1 Compressive strength

24 hour

36 hour

3 days

7 days

14 days

28 days

56 days

others if any ( Compressive strength )

2 Durability requirement

RCPT

Water Permability

Other ( )
Date :-

e.g. Column, Beam, Slab, Raft or Footing etc.

e.g. P.C.C. etc.

Notes :-
1) It is advisable to use PSC or OPC+GGBFS or OPC+Flyash+GGBFS
combo with min. 50% replacements of GGBFS where chlorides
encountered with sulphates in soil or ground water.
2) In other situations, OPC+Flyash combo can also be used.
3) For raft, concrete can be design for 56 days or 90 days strength.

ot exceed 70 oC.
mass should not exceed 20 oC.
sign concrete for 56 days or 90 days strength.

or normal density concrete (i.e. other than light or high density concrete).

Maximum value out of below conditions :-


1) Refer geotechnical inspection report for sub structure only.
2) Refer IS 456 Table 4 for sub structure only.
3) Refer IS 456 Table 5 & 6.

Maximum value out of below conditions :-


1) Refer geotechnical inspection report for sub structure only.
2) Refer IS 456 Table 4 for sub structure only.
3) Refer IS 456 Table 5 & 6.

t exceed :-
stressed concrete,
concrete &
ning embeded metal.
ot exceed 4% by mass of cement in mix.
If requirement not justified or mentioned "As per QA/QC" then
following required properties to be consider:-

Slump Flow

200 +/-25mm 650 +/- 50 mm

200 +/-25mm 650 +/- 50 mm

150 +/- 25mm 500 +/- 50mm

3 hours

If requirement not justified or mentioned "As per QA/QC" then


following required properties to be consider:-

NA

NA

NA

Min. 70%

NA

Min. 100%

NA

If requiement not mentioned then follow below conditions :-

For Sub structures For Superstructures

Less than 1000 Coulomb Not more than 1500 Coulomb

Max. 15 mm Max. 20 mm